Material Notes:
Formula: CH2FCF3; Name: 1,1,1,2 Tetrafluoroethane. Replaces CFC 12, R 500. Domestic refrigeration, commercial and automotive air-conditioning, polystyrene and polyurethanes foams, and pharmaceutical aerosol propellant. Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.21 g/cc

@Temperature 25.0 °C
0.0437 lb/in³

@Temperature 77.0 °F
Liquid
Molecular Weight 102 g/mol
102 g/mol
Vapor Pressure 6.66 bar

@Temperature 25.0 °C
5000 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Heat of Vaporization 217 J/g
93.4 BTU/lb
at Boiling Point
Melting Point -101 °C
-150 °F
at 1.013 bar
Boiling Point -26.2 °C
-15.2 °F
at 1.013 bar
Chemical Properties Metric English Comments
Critical Pressure 40.67 bar
30510 torr
Critical Temperature 101.1 °C
214.0 °F
Critical Density 0.510 g/cc
0.0184 lb/in³
Descriptive Properties Value Comments
Flammability Range (vol%) None
Ozone Depletion Potential 0
Based on CFC11 = 1.0
Toxicity Level 1000 ppm
Allowed limit in work places, values suggested by AIHA (American Industrial Hygiene Association).
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved