Solvay Specialty Polymers KetaSpire® KT-880 GF20 Polyetheretherketone (PEEK), 20% Glass Fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer Solvay Specialty Polymers
Trade Name KetaSpire®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers KetaSpire® KT-880 GF20 Polyetheretherketone (PEEK), 20% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KetaSpire® KT-880 GF20 is a high flow, 20% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire® PEEK resin. The glass fiber content is optimized to provide a balance of strength and stiffness with toughness-related properties, such as impact resistance and elongation at break. This level of reinforcement also affords greater mechanical robustness in structural applications, particularly those with service temperatures approaching 300°C (572°F).Features: Autoclave Sterilizable; Biocompatible; E-beam Sterilizable; Ethylene Oxide Sterilizable; Fatigue Resistant; Flame Retardant; Good Chemical Resistance; Good Dimensional Stability; Good Sterilizability; Heat Sterilizable; High Flow; High Heat Resistance; High Stiffness; High Strength; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam SterilizableUses: Aircraft Applications; Automotive Applications; Connectors; Dental Applications; Electrical/Electronic Applications; Film; Hospital Goods; Industrial Applications; Medical Devices; Medical/Healthcare Applications; Oil/Gas Applications; Pump Parts; Seals; Surgical InstrumentsAdditional Properties: Ash Content - ISO 3451-1 20 %; Modulus of Elasticity - ISO 527 8.24 GPaInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Filler Content 20 %
20 %
Glass Fiber
Water Absorption 0.022 %

@Time 86400 sec
0.022 %

@Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 162 MPa
23500 psi
ISO 527-2
Elongation at Break 3.5 %
3.5 %
Type 1A, 5 mm/min; ISO 527-2
Flexural Strength 238 MPa
34500 psi
ISO 178
Flexural Modulus 7.72 GPa
1120 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 345 °C
653 °F
ISO 11357-3
Processing Properties Metric English Comments
Rear Barrel Temperature 365 °C
689 °F
Middle Barrel Temperature 371 °C
700 °F
Front Barrel Temperature 377 °C
711 °F
Nozzle Temperature 382 °C
720 °F
Mold Temperature 177 - 204 °C
351 - 399 °F
Drying Temperature 150 °C

@Time 14400 sec
302 °F

@Time 4.00 hour
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Tan
Form Pellets
Injection Rate Fast
Processing Technique Injection Molding
Screw Compression Ratio 2.5:1.0 to 3.5:1.0