Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Kalix® 9945 HFFR Polyamide, High Performance (HPPA), 45% Glass Fiber

Category Polymer , Thermoplastic , Nylon
Manufacturer Solvay Specialty Polymers
Trade Name Kalix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Kalix® 9945 HFFR Polyamide, High Performance (HPPA), 45% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Kalix® 9945 HFFR is a 45% glass-fiber reinforced, halogen-free flame retardant High Performance Polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties, excellent surface quality and excellent flammability rating.Features: Fast Molding Cycle; Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; High Flow; High Stiffness; High Strength; Hot Water Moldability; Low Warpage; Paintable; PlatableUses: Cell Phones; Electrical Parts; Electrical/Electronic Applications; Thin-walled PartsInjection Molding Notes: Kalix® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Kalix® resins be dried prior to molding.Additional Properties: Flexural Strain at Break - ISO 178 2.5 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ISO 1183
Filler Content 45 %
45 %
Glass Fiber
Linear Mold Shrinkage, Flow 0.0012 cm/cm
0.0012 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0028 cm/cm
0.0028 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 190 MPa
27600 psi
ISO 527-2
Elongation at Break 1.9 %
1.9 %
ISO 527-2
Tensile Modulus 17.0 GPa
2470 ksi
ISO 527-2
Flexural Strength 280 MPa

@Strain 3.50 %
40600 psi

@Strain 3.50 %
ISO 178
Flexural Modulus 15.0 GPa
2180 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 257 °C
495 °F
HDT B; Unannealed; ISO 75-2/B
Flammability, UL94 V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
Electrical Properties Metric English Comments
Dielectric Constant 4.2

@Frequency 2.40e+9 Hz
4.2

@Frequency 2.40e+9 Hz
ASTM D2520
Dissipation Factor 0.010

@Frequency 2.40e+9 Hz
0.010

@Frequency 2.40e+9 Hz
Method B; ASTM D2520
Processing Properties Metric English Comments
Rear Barrel Temperature 265 - 270 °C
509 - 518 °F
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Melt Temperature 280 - 290 °C
536 - 554 °F
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Drying Temperature 80.0 °C

@Time 14400 - 43200 sec
176 °F

@Time 4.00 - 12.0 hour
Moisture Content <= 0.090 %
<= 0.090 %
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color Black; Colors; Natural
Form Pellets
Part Marking Code >PAMXD6/66-GF45<
ISO 11469
Processing Technique Injection Molding; Water-Heated Mold Injection Molding