Solvay Specialty Polymers Hyflon® PFA P7010 Perfluoroalkoxy (PFA)  (Unverified Data**)

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Hyflon® PFA P7010 Perfluoroalkoxy (PFA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hyflon® PFA P7010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in antistick applications. Hyflon® PFA P7010 exhibits very low surface energy, very low coefficient of friction and excellent thermal and flame resistance Additionally Hyflon® PFA P7010 coatings show excellent smooth surface finish, outstanding antistick behavior and can maintain performance over a wide temperature range. Main features of Hyflon® PFA P7010 include: - Very low surface energy - Excellent antistick behaviour - Very low coefficient of friction - Very good surface finish - Outstanding thermal resistanceAdditional Information: Processing - Hyflon® PFA P7010 is intended as a topcoat material to apply to primered substrates. It can be processed using normal electrostatic powder coating techniques. Generally the procedure involves substrate preparation, coating, baking and cooling. - Hyflon® PFA P7010 can be used neat and without any further formulation. Several passes may be required to obtain the desired PFA load and build up coating thickness without defects. - Substrate preparation, gun parameters such as voltage and both oven temperature and time must all be well controlled to achieve defect free coated items. Storage and Handling - Hyflon® melt processable fluoropolymer resins can be stored without shelf life issues when kept in a clean and dry area at ambient temperatures. Opened containers should be tightly resealed to prevent any contamination. Safety and Toxicology - Before using Hyflon® melt processable fluoropolymer resins consult the product Material Safety Data Sheet and follow all label directions and handling precautions. - As with all fluoropolymer materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapor or fumes. - See Material Safety Data Sheet for detailed advice on waste disposal methods. Packaging - Hyflon® PFA P7010 is packaged in 10kg non returnable drums. Each drum has two bags liner made of polyethylene resin.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM D792
Particle Size 25 µm
25 µm
Laser Diffraction; Internal Method
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 300 - 310 °C
572 - 590 °F
ASTM D4591
Descriptive Properties Value Comments
Appearance Clear/Transparent
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Good Surface Finish
Good Thermal Stability
Low Friction
Semi Crystalline
Forms Powder
Generic PFA
Processing Method Coating
Uses Coating Applications