FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity indices.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.91 g/cc
0.0690 lb/in³
ASTM D891
Viscosity Measurement 135
135
Viscosity Index; ASTM D2270
Kinematic Viscosity 1300 cSt

@Temperature 20.0 °C
1300 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 345 cSt
345 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 33 cSt
33 cSt
ASTM D445
Molecular Weight 6250 g/mol
6250 g/mol
Evaporation Loss 0.50 %
0.50 %
22 hrs. at 149°C; ASTM 2595
1.2 %
1.2 %
22 hrs. at 204°C; ASTM 2595
Surface Tension 24 dynes/cm
24 dynes/cm
ASTM D1331
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 124 kg
273 lb (mass)
Mean Hertz Load; IP 239
282 kg
622 lb (mass)
Init. Seiz. Load; IP 239
708 kg
1560 lb (mass)
Welding Load; IP 239
Four Ball Wear 0.900 mm
0.0354 in
Avg. scar diameter; ASTM D4172
Thermal Properties Metric English Comments
Pour Point -25.0 °C
-13.0 °F
ASTM D97
Descriptive Properties Value Comments
Approximate ISO Grade 320
Copyright © lookpolymers.com All Rights Reserved