Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers FOMBLIN® YPL1500 PFPE Lubricant

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® YPL1500 PFPE Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity indices.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.91 g/cc
0.0690 lb/in³
ASTM D891
Viscosity Measurement 135
135
Viscosity Index; ASTM D2270
Kinematic Viscosity 1500 cSt

@Temperature 20.0 °C
1500 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 420 cSt
420 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
ASTM D445
Molecular Weight 6600 g/mol
6600 g/mol
Evaporation Loss 0.30 %
0.30 %
22 hrs. at 149°C; ASTM 2595
0.90 %
0.90 %
22 hrs. at 204°C; ASTM 2595
Surface Tension 24 dynes/cm
24 dynes/cm
ASTM D1331
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 126 kg
278 lb (mass)
Mean Hertz Load; IP 239
355 kg
783 lb (mass)
Init. Seiz. Load; IP 239
708 kg
1560 lb (mass)
Welding Load; IP 239
Four Ball Wear 0.950 mm
0.0374 in
Avg. scar diameter; ASTM D4172
Thermal Properties Metric English Comments
Pour Point -25.0 °C
-13.0 °F
ASTM D97
Descriptive Properties Value Comments
Approximate ISO Grade 460
Copyright © lookpolymers.com All Rights Reserved