Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers FOMBLIN® Y H-VAC 40/11 PFPE Pump Oil

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® Y H-VAC 40/11 PFPE Pump Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and oxygen atoms, the PFPEs have exceptional properties such as: low vapor pressure; chemical inertness; non-flammability; high thermal stability; no flash or fire point; low toxicity; excellent compatibility with metals, plastics, elastomers; low volatility; good aqueous and non-aqueous solvent resistance; high dielectric properties; low surface tension; good radiation stability; and environmentally friendly-do not damage the ozone.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.91 g/cc
0.0690 lb/in³
ASTM D891
Kinematic Viscosity 474 cSt

@Temperature 20.0 °C
474 cSt

@Temperature 68.0 °F
ASTM D445
Molecular Weight 4100 g/mol
4100 g/mol
Vapor Pressure 8.00e-15 bar

@Temperature 20.0 °C
6.00e-12 torr

@Temperature 68.0 °F
Knudsen
4.00e-10 bar

@Temperature 100 °C
3.00e-7 torr

@Temperature 212 °F
Knudsen
Thermal Properties Metric English Comments
Heat of Vaporization 29.3 J/g

@Temperature 200 °C
12.6 BTU/lb

@Temperature 392 °F
Pour Point -32.0 °C
-25.6 °F
ASTM D97
Optical Properties Metric English Comments
Refractive Index 1.301
1.301
n<sub>0</sub><sup>20</sup>
Users viewing this material also viewed the following: