Solvay Specialty Polymers FOMBLIN® M100 PFPE Lubricant

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® M100 PFPE Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.87 g/cc
0.0676 lb/in³
ASTM D891
Viscosity Measurement 375
375
Viscosity Index; ASTM D2270
Kinematic Viscosity 1300 cSt

@Temperature 20.0 °C
1300 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 700 cSt
700 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 200 cSt
200 cSt
ASTM D445
Molecular Weight 12500 g/mol
12500 g/mol
Evaporation Loss 0.30 %
0.30 %
22 hrs. at 204°C; ASTM 2595
Surface Tension 25 dynes/cm
25 dynes/cm
ASTM D1331
Thermal Properties Metric English Comments
Pour Point -50.0 °C
-58.0 °F
ASTM D97