Material Notes:
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefin base containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution, toxic and corrosive gases and dark smoke emission. This material complies with RoHS requirements.Features: Crosslinkable; Flame Retardant; Fuel Resistant; Halogen Free; Low Smoke Emission; Low Toxicity; Oil Resistant; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsAdditional Properties: Bending Test - IEC 60811 (-40°C): No cracks; Calorific Potential - ISO 1716 18.3 MJ/kg; Collar Temperature - 150 to 170 °C; Corrosive Gas in Smoke - IEC 60754-2 < 10.0 µS/mm; Corrosive Gas in Smoke - IEC 60754-2 > 4.30; Halogenidric Acid Emissions - IEC 60754-1 < 0.10 %; Head Temperature - 150 to 170 °C; Hot Pressure Test - IEC 60811 (100°C): < 50 %; Hot Set - IEC 60811 60 %; Hot Set - IEC 60811 0.0 %; Insulation Resistance Constant - IEC 60502 (20°C): 3500 Mohm·km; Insulation Resistance Constant - IEC 60502 (90°C): 500 Mohm·km; Temperature Index (Burning) - NES 715 300 °C; Water Absorption - IEC 60811 (70°C): 0.230 mg/cm²; Water Absorption - IEC 60811 (100°C): 0.780 mg/cm²Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded, 10% Igepal; ASTM D1693
Melt Flow 6.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ISO 868
Tensile Strength at Break 11.5 MPa
1670 psi
ASTM D638
Elongation at Break 180 %
180 %
ASTM D638
Thermal Properties Metric English Comments
Oxygen Index 38 %
38 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.40e+14 ohm-cm

@Temperature 90.0 °C
1.40e+14 ohm-cm

@Temperature 194 °F
ASTM D257
9.50e+14 ohm-cm

@Temperature 20.0 °C
9.50e+14 ohm-cm

@Temperature 68.0 °F
ASTM D257
Processing Properties Metric English Comments
Zone 1 130 - 150 °C
266 - 302 °F
Zone 2 140 - 160 °C
284 - 320 °F
Zone 3 140 - 160 °C
284 - 320 °F
Zone 4 140 - 170 °C
284 - 338 °F
Die Cooling Temperature 160 - 200 °C
320 - 392 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: