Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, at 50% RH  (disc

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), Mineral Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, at 50% RH  (disc.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offers excellent dimensional stability and chemical resistance, good mechanical properties and low warpage, and moisture absorption.This material is readily injection molded using conventional equipment and methods.Information provided by Solvay Advanced Polymers
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.20 %
0.20 %
24 hours; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 71.0 MPa
10300 psi
ASTM D638
Elongation at Yield 2.5 %
2.5 %
ASTM D638
Tensile Modulus 5.80 GPa
841 ksi
ASTM D638
Flexural Strength 135 MPa
19600 psi
ASTM D790
Flexural Modulus 5.50 GPa
798 ksi
ASTM D790
Shear Strength 69.0 MPa
10000 psi
ASTM D732
Izod Impact, Notched 0.650 J/cm
1.22 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 313 °C
595 °F
ASTM D3418
Users viewing this material also viewed the following: