Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Heat Resistance; High Stiffness; High Strength; High Temperature Strength; Low Moisture AbsorptionUses: Automotive Electronics; Connectors; Electrical Parts; Electrical/Electronic ApplicationsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
Dry; ISO 1183
Filler Content 33 %
33 %
Glass Fiber
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
Dry
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Dry; ASTM D955
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+14 ohm-cm
5.00e+14 ohm-cm
ASTM D257
Dielectric Constant 3.4

@Frequency 1.00e+6 Hz
3.4

@Frequency 1.00e+6 Hz
ASTM D150
4.3

@Frequency 60.0 Hz
4.3

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
ASTM D149
Dissipation Factor 0.019

@Frequency 1.00e+6 Hz
0.019

@Frequency 1.00e+6 Hz
ASTM D150
0.020

@Frequency 60.0 Hz
0.020

@Frequency 60.0 Hz
ASTM D150
Comparative Tracking Index 600 V
600 V
UL 746
High Voltage Arc-Tracking Rate, HVTR 18.0 mm/min
0.709 in/min
UL 746
Processing Properties Metric English Comments
Rear Barrel Temperature 320 - 330 °C
608 - 626 °F
Middle Barrel Temperature 320 - 330 °C
608 - 626 °F
Front Barrel Temperature 327 - 335 °C
621 - 635 °F
Melt Temperature 330 - 345 °C
626 - 653 °F
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Moisture Content 0.030 - 0.060 %
0.030 - 0.060 %
Suggested Max
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Processing Technique Injection Molding