Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® A-6625 HS BK324 Polyphthalamide, 25% carbon/glass fiber, ESD grade  (discont

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), Carbon Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® A-6625 HS BK324 Polyphthalamide, 25% carbon/glass fiber, ESD grade  (discont.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel A-6625 HS BK324 is a 25% carbon and glass-fiber-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material is well suited for fuel systems applications requiring low permeation, low swell, and high thermal resistance. It can also be used for components of electrical/electronic systems requiring high strength and stiffness, as well as static charge dissipation. Amodel A-6625 HS BK324 resin provides low moisture absorption, excellent dimensional stability and has creep resistance superior to other electrostatic dissipative materials. This resin can be easily processed by injection molding using water-cooled molds, conventional equipment, and methods.Data for dry-as-molded samples.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Water Absorption 0.25 %
0.25 %
24 hrs; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 135 MPa
19600 psi
ISO 527
Elongation at Break 4.0 %
4.0 %
ISO 527
Tensile Modulus 10.0 GPa
1450 ksi
ISO 527
Flexural Strength 200 MPa
29000 psi
ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
ISO 178
Charpy Impact Unnotched 8.00 J/cm²

@Temperature -40.0 °C
38.1 ft-lb/in²

@Temperature -40.0 °F
ISO 179
Charpy Impact, Notched 1.20 J/cm²

@Temperature -40.0 °C
5.71 ft-lb/in²

@Temperature -40.0 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 295 °C
563 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ISO 75
Glass Transition Temp, Tg 88.0 °C
190 °F
Processing Properties Metric English Comments
Melt Temperature 320 - 330 °C
608 - 626 °F
Injection Molding
Mold Temperature 65.0 - 93.0 °C
149 - 199 °F
Drying Temperature 90.0 - 135 °C
194 - 275 °F
Moisture Content 0.030 - 0.060 %
0.030 - 0.060 %
Users viewing this material also viewed the following: