Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength and stiffness over a broad temperature range. It also exhibits low moisture absorption, excellent chemical resistance and excellent electrical properties.Features: Good Chemical Resistance; Good Creep Resistance; Good Flow; Good Stiffness; Heat Stabilized; High Heat Resistance; High Stiffness; High Strength; Hot Water Moldability; Low Moisture AbsorptionUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; Electrical Housing; Electrical/Electronic Applications; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D6779 PA101G35; GM GMP.PPA.021 Color: Black; GM GMP.PPA.021 Color: Natural; GM GMW16362P-PPA-GF35 Color: BlackInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
Dry; ISO 1183
Filler Content 35 %
35 %
Glass Fiber
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Dry
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
Dry; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 176 MPa
25500 psi
ASTM D638
Elongation at Break 2.1 %
2.1 %
ASTM D638
Tensile Modulus 12.2 GPa
1770 ksi
ASTM D638
Flexural Strength 249 MPa
36100 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Shear Strength 73.8 MPa
10700 psi
ASTM D732
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 310 °C
590 °F
Dry; ISO 11357-3
310 °C
590 °F
Dry; DSC
Processing Properties Metric English Comments
Rear Barrel Temperature 316 - 321 °C
601 - 610 °F
Front Barrel Temperature 327 - 332 °C
621 - 630 °F
Melt Temperature 321 - 335 °C
610 - 635 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Moisture Content <= 0.045 %
<= 0.045 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black
Form Pellets
Processing Technique Water-Heated Mold Injection Molding