Solvay Specialty Polymers Algoflon® 15GL+3Mos PTFE; Glass Fiber/Molybdenum Disulphide Filled  (discontinued **

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Algoflon® 15GL+3Mos PTFE; Glass Fiber/Molybdenum Disulphide Filled  (discontinued **.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.15 wt.% Glass Fiber + 3 wt.% MoS2. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost no moisture absorption, low friction coefficient, and is nonflammable.
Physical Properties Metric English Comments
Density 2.27 g/cc
0.0820 lb/in³
ASTM D792
Apparent Bulk Density 0.510 g/cc
0.0184 lb/in³
ASTM D4894
Linear Mold Shrinkage 0.024 cm/cm
0.024 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
Tensile Strength, Ultimate 27.0 MPa
3920 psi
ASTM D638
Elongation at Break 270 %
270 %
ASTM D638
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Coefficient of Friction, Static 0.080
0.080
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 160 µm/m-°C

@Temperature 23.0 - 250 °C
88.9 µin/in-°F

@Temperature 73.4 - 482 °F
ASTM D696
Maximum Service Temperature, Air 260 °C
500 °F