Material Notes:
Sodium Isopropyl Naphthalene Sulfonate. Multipurpose, low foaming wetting agent.Identification: DIALKYL NAPHTHALENE SULPHONATE SODIUM SALTCAS: 1322 – 93 -6Solubility: Soluble in water. Insoluble in aromatic and polar solvents.Available in: Asia Pacific, Europe, Latin America and North America Applications: Wetting agent.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 0.400 g/cc
0.0145 lb/in³
pH 7.0 - 9.0
7.0 - 9.0
5% aq. Sol.; 540MA3C1E
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 5.0 %
<= 5.0 %
K. Fischer; 540MA3C09
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Fineness powder
Composition Active
0.7
Ionic Charge Anionic