Material Notes:
Description: Highly effective white oil defoamer for latex processing.Available in: Asia Pacific, Europe, Latin America and North America.Solubility: Dispersible in water. Soluble in most polar and aromatic solvents. Applications: Antifoaming and cleaner in metal working.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
pH 5.0 - 7.0
5.0 - 7.0
1% in water; RPG02
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear liquid
RPG31
Cloud Point 32-38°C
RPG08
Composition Active
1
Ionic Charge Nonionic