Solvay RHODOLINE® DF 540 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODOLINE® DF 540 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Highly effective white oil defoamer for latex processing.Identification: DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© DF 540 is a general purpose silicone-free, high active type defoamer that is recommended for use in waterborne resins and adhesives. RHODOLINE© DF 540 is dispersible in water and can be used as received or diluted prior to use. As a starting point use in the lab evaluations of the formulation, a 0.05 – 0.2 % usage level is suggested.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.870 - 0.930 g/cc
0.0314 - 0.0336 lb/in³
RP-1008
Viscosity 350 - 700 cP
350 - 700 cP
LVTDV-I-A3 V50; RP-0596
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Opaque Liquid
RP-0064