Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay RHODOLINE® 581B Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODOLINE® 581B Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Mineral oil defoamers for high PVC systems Chemical Name: DEFOAMERCAS: 64742-47-8Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility(2% in DI Water): Coarse Dispersion, RP-0547Applications: The amount of RHODOLINE© 581B required for a specific application should be determined in each case, because of the variance in factors creating foam. Since severe foaming is often controlled with 0.1% RHODOLINE© 581B, this concentration is suggested as a starting point. Make subsequent adjustments to dilute or increase the concentration to the most efficient and economical strength. In some applications, higher concentrations will be needed to obtain the desired persistence. RHODOLINE© 581B will separate on prolonged standing; therefore, it should be mixed well before using. For greater efficiency and stability, an emulsion pre-mix is suggested. This is prepared by adding with mixing one part of water to two parts of RHODOLINE© 581B. More dilute emulsions may be used; however, they require more frequent mixing before use.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.790 - 0.830 g/cc
0.0285 - 0.0300 lb/in³
RP-17617
pH 4.5 - 6.5
4.5 - 6.5
2% Solution; RP-0420
6.0 - 6.7
6.0 - 6.7
Acid Value; RP-9187
Viscosity <= 1000 cP
<= 1000 cP
#3 sp @ 60 rpm; RP-0596
Brookfield Viscosity 500 cP
500 cP
30 rpm
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Hazy Cream Liquid
RP-0064
Users viewing this material also viewed the following: