Solvay RHODOLINE® 286N Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODOLINE® 286N Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hydrophilic copolymer dispersant. Semi gloss to high gloss, TiO2 slurry, interior/exterior, low foam.Identification: AMMONIUM POLYACRYLATE COPOLYMER SOLUTIONAvailable in: North AmericaApplications: RHODOLINE© 286N is an acrylic, non-foaming, multi-purpose anionic dispersant. Use RHODOLINE© 286N at concentration of 2 to 8 pounds per 100 gallons of finished paint. The optimum use level of RHODOLINE© 286N in each formulation may be determined by running a dispersant demand curve.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Solids Content 49 - 51 %

@Temperature 130 °C,
Time 3600 sec
49 - 51 %

@Temperature 266 °F,
Time 1.00 hour
Oven, 0.5 g; RP-0540
Volatile Organic Compounds (VOC) Content <= 1.0 g/l
<= 1.0 g/l
ASTM D2369
pH 6.5 - 7.3
6.5 - 7.3
RP-0420
Viscosity 50 - 200 cP
50 - 200 cP
#2 sp @ 30 rpm; RP-0596
Molecular Weight 2700 g/mol
2700 g/mol
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear, Colorless to yellow
RP-0064