Solvay RHODOCLEAN® EFC Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODOCLEAN® EFC Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: ETHOXYL-PROPOXYL TERPENECAS: 174955 – 61 – 4Available in: Asia Pacific, Europe, Latin America and North America Solubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Applications: Low foam detergent with excellent ecotox profile and high biodegradability. Used in all kinds of cleaning applications.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
pH 6.0 - 8.0
6.0 - 8.0
1% in water; RPG02
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear liquid
RPG31
Cloud Point 32-38°C
1% in water, RPG08
Composition Active
1
Ionic Charge Nonionic