Material Notes:
Rhodicare® S 100% natural thickening biopolymer delivering viscosity and suspension/stabilization properties to cosmetic formulations. Rhodicare® S displays a high hydration rate. Approved for Ecocert.C.T.F.A. /I.N.C.I. Name: Xanthan GumCAS: 11138 - 66 – 2EINECS: 234 – 394-2Recommended use level: 0.2 - 1%.Soluble in waterCompatible with Non-ionic, anionic and amphoteric surfactants.Applications: Sodium salt of an anionic high molecular weight hetero-polysaccharide produced by pure culture fermentation of Xanthomonas campestris, purified by recovery with isopropanol, dried and milled.Thickening and stabilizing hydrocolloid giving aqueous solutions of high viscosity and high yield value even at low concentrations, not affected by temperature. Pseudo-plastic non thixotropic behaviour. Effective suspending and stabilizing agent for multi-phasic systems: aqueous suspensions, emulsions and foams, easily sprayable, flowable, pumpable (creams and lotions, toothpastes…). Thickening agent for creams, suspensions, shampoos, gels; synergistic effect with galactomannanes, glucomannanes. Anti-syneresis agent, reduces gel exudation.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
Particle Size 180 µm
180 µm
95 min, 80 mesh; TI-2087
250 µm
250 µm
99.5 min, 60 mesh; TI-2087
pH 6.0 - 8.0
6.0 - 8.0
1% aqueous sol.; TI-2076
Brookfield Viscosity 1200 - 1600 cP
1200 - 1600 cP
1% KCl, LVT, 60 rpm, spindle 3; TI-1110
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Fine powder
Color Creamy white
Composition 2-Propanol
<750 ppm, TI-2105
Arsenic as As
<3 ppm, USP
Ash
6.5-16%, TI-0130
Entero-bacteria & other Gram Neg.
Absence in 1g, TI-2185
Heavy metal as Pb
<10 ppm, TI-2109
Pseudomonas aeruginosa
Absence in 1g, TI-2073
Staphylococcus aureus
Absence in 1g, TI-2073
Total viable aerobic count
<500 cfu/g, TI-2070
Yeasts and moulds
<100 cfu/g, TI-2071
Loss on drying <13%