Material Notes:
Description: Rhodicare® CFT is Cellulase-free clear grade of Xanthan Gum, it is recommended when associated with cellulose-based polymers. Approved for Ecocert. It is excellent anionic bio-polymer viscosity modifier and stabilizer and in conjunction with nonionic guars exhibits excellent suspending properties.C.T.F.A. /I.N.C.I. Name: XANTHAN GUMCAS: 11138 - 66 – 2EINECS: 234 - 394Recommended use level : 0.2 - 1%.Soluble in waterCompatible with Non-ionic, anionic and amphoteric surfactants.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Sodium salt of an anionic high molecular weight hetero-polysaccharide produced by pure culture fermentation of Xanthomonas campestris, purified by recovery with isopropanol, dried and milled. Thickening and stabilizing hydrocolloid giving aqueous solutions of high viscosity and high yield value even at low concentrations, not affected by temperature. Pseudo-plastic non thixotropic behaviour. Effective suspending and stabilizing agent for multi-phasic systems : aqueous suspensions, emulsions and foams, easily sprayable, flowable, pumpable (creams and lotions, toothpastes…) Thickening agent for creams, suspensions, shampoos, gels ; synergistic effect with galactomannanes, glucomannanes. Anti-syneresis agent, reduces gel exudation. Finished products using RHODICARE CFT keep original clarity. Compatible with cellulose derivatives in toothpaste formulations.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
Particle Size 180 µm
180 µm
95% min, 80 mesh; TI-2087
pH 6.0 - 8.0
6.0 - 8.0
1% aqueous sol.; TI-2078
Brookfield Viscosity 1400 - 1700 cP
1400 - 1700 cP
1% KCl, LVT, 60 rpm, spindle 3; TI-1110
Optical Properties Metric English Comments
Transmission, Visible >= 80 %

@Wavelength 650 nm
>= 80 %

@Wavelength 650 nm
aqueous sol. 0.5%, cell 1 cm; TI-2081
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Fine powder
Color Creamy white
Composition 2-Propanol
<500 ppm, TI-2105
Arsenic as As
<1 ppm, USP
Ash
6.5-16%, TI-0130-2
Entero-bacteria & other Gram Neg.
Absence in 1g, TI-2101
Esherichia coli
Absence in 5g, TI-2074
Heavy metal as Pb
<5 ppm, TI-2109
Lead as Pb
<1 ppm, USP
Pseudomonas aeruginosa
Absence in 1g, TI-2073
Salmonella species
Absence in 25g, TI-2074
Staphylococcus aureus
Absence in 1g, TI-2073
Total viable aerobic count
<500 cfu/g, TI-2070
Yeasts and moulds
<100 cfu/g, TI-2071
Loss on drying 7-13%
TI-0515