Solvay RHODASURF® TB-970/FLK Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODASURF® TB-970/FLK Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rhodasurf® TB- 970/FLK is highly water soluble APE-free non ionic surfactant. It is in flake form and is good foam control agent, stabilizer, emulsifier, detergent, and wetting agent.Chemical Name: ALCOHOLS, C12-20, ETHOXYLATEDCAS: 68526-94-3 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODASURF© TB-970/FLK is a highly water soluble, APE-free nonionic surfactant that is used for emulsion polymerization of acrylic, vinyl acetate, and vinyl-acrylic systems.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Flakes
@ 25°C, RP-0064
Liquid
@ 60°C, RP-0064
Color <20
APHA, 5% Solution, RP-0134
Ionic Charge Nonionic
Neutralization Number <1.0 mg KOH/g
pH 7, RP-0343
Solidification Point 51-55°C
RP-0524