Solvay RHODASURF® T 50 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODASURF® T 50 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: WATER SOLUTION OF ETHOXYLATED OLEYL – CETYL ALCOHOLCAS: 68920 – 66 – 1 ; 7732 – 18 – 5Solubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Fatty alcohol ethoxylate with a HLB of 16. Detergent, emulsifier, wetting agent for metal cleaning liquid and powder formulationInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
pH 6.0 - 7.5
6.0 - 7.5
2% in water; RPG02
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content 50 - 52 %
50 - 52 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Limpid liquid
RPG31
Cloud Point 43-47°C
1% solution NaCl 5%, RPG08
Color <100 HU
RPG23
Composition Active
0.49
Ionic Charge Nonionic