Solvay RHODASURF® ROX Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODASURF® ROX Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: ETHOXYLATED FATTY ALCOHOLCAS: 24938 – 91 – 8Solubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Agrochemical formulations: Wetting agent for agrochemical formulations. Industrial formulations: Emulsifier and wetting agent for industrial formulations. Also used to emulsify silicone oils. Metal treatment: Branched alcohol ethoxylate with a HLB of 13. Emulsifier and wetting agent for industrial formulations. Also used to emulsify silicone oils. Polymer system specialties: Co-emulsifier in the emulsion polymerization or post-added to increase shelf stability.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
pH 5.0 - 7.0
5.0 - 7.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content 14 - 16 %
14 - 16 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Limpid liquid
RPG31
Cloud Point 43-47°C
1% aq. Sol., RPG08
Color <100 HU
RPG23
Composition Active
0.85
Ionic Charge Nonionic