Solvay RHODASURF® ID 030 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODASURF® ID 030 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: SYNTHESIS FATTY ALCOHOL ETHOXYLATEDCAS: 26183 – 52 – 8Solublility: Soluble in chlorhydric acid, mineral oils, alcohols and aromatic hydrocarbons. Insoluble in water.Available in: Asia Pacific, Europe, Latin America and North America Applications: Emulsifier for mineral oil in for water expandable metalworking fluids. Surfactant for cleaning formulationsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
pH 5.0 - 8.0
5.0 - 8.0
5% aq. Sol.; 540MA3C1E
Chemical Properties Metric English Comments
Total Acid Number 190
190
[mg KOH/g]
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Liquid
540MA3C1F
Cloud Point 51-55°C
DIN 53917
Color <2
Iodine color at 50°C, 540MA3C13
Composition Active
1
HLB number 9
Ionic Charge Nonionic
Setting point <5°C