Solvay RHODASURF® BC-840 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODASURF® BC-840 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: TRIDECYL ALCOHOL ETHOXYLATEDCAS: 78330-21-9Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODASURF BC-840 is used for the following applications: foam stabilizer and detergency booster for alkylarylsulfonates, solubilizer for salt-free alkylarylsulfonates, component of light and heavy duty high foaming detergent formulations, detergent and wetting agent for use with strong alkalis. RHODASURF BC-840 is a surfactant for high temperature detergency, wetting agent in high concentrations of electrolytes. It is a stabilizer and emulsifier for synthetic lattices and aromatic solvents, fats, essential oils, and waxes.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.01 - 1.04 g/cc
0.0365 - 0.0376 lb/in³
Solids Content 100 %
100 %
pH 6.0 - 8.0
6.0 - 8.0
0.1
Thermal Properties Metric English Comments
Pour Point 33.0 - 40.0 °C
91.4 - 104 °F
Flash Point >= 93.3 °C
>= 200 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Pourable Liquid
Above melting point, RP-0064
Waxy Paste
RP-0064
Cloud Point 80-85°C
2% in 5% Salt Sol., RP-0732
Color <100
APHA, RP-0134
HLB number 15.4
Ionic Charge Nonionic
Moles of Ethylene Oxide 15
Neutralization Number <0.5 mg KOH/g
pH 7, RP-0343
Odor Mild, pleasant