Solvay RHODASURF® 91-6 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODASURF® 91-6 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: EYHOXYLATED C9-11 ALCOHOLSCAS: 68439-46-3Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODASURF 91-6 is an excellent wetting agent and emulsifier for use in household all purpose cleaners, laundry products, industrial metal cleaners, floor cleaners, wax strippers, car wash and many other applications. RHODASURF 91-6 provides excellent detergency and exhibits a biodegradable profile.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH 5.5 - 7.5
5.5 - 7.5
1% Solution; RP-0420
Processing Properties Metric English Comments
Moisture Content <= 0.30 %
<= 0.30 %
Karl Fisher; RP-0327
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear to slightly hazy liquid
RP-0064
Cloud Point 47-58°C
1% in DW, RP-0130
Color <50
APHA, RP-0134
Moles of Ethylene Oxide 5.5-6.5
RP-0245