Solvay RHODAQUAT® M-242B/99 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAQUAT® M-242B/99 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rhodaquat® M-242B/99 is high purity cationic surfactant A free flowing crystalline powder has unique property of static and tangling elimination, imparting soft and elegant feel to hair thus enabling preparation of premium quality cream rinse hair conditionersChemical Name: CETRYLTRIMETHYLAMMONIUM BROMIDECAS: 57-09-0 Use Concentration: 0.1-2.0%Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODAQUAT® M-242B/99 is a high purity cationic surfactant ideally suited for use in the preparation of premium quality crème rinse conditioners. A free flowing crystalline powder, RHODAQUAT® M-242B/99 eliminates static and tangling while imparting a soft, elegant feel to the hair.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.500 g/cc
0.0181 lb/in³
Thermal Properties Metric English Comments
Melting Point 230 °C
446 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month
60.0 Month
Descriptive Properties Value Comments
Appearance White Free Flowing Powder
RP-0064
Assay 99-101%, MW364.5, RP-0032
Composition Amine Hydrobromide
<0.12%, MW 350, RP-0990
Free Amine
<0.1%, MW 270, RP-0990
Sulphate Ash
<0.5%, RP-0929
Ionic Charge Cationic