Solvay RHODAPHOSE® TRIETHYL PHOSPHONOACETATE Phosphorus Derivative

Category Fluid
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAPHOSE® TRIETHYL PHOSPHONOACETATE Phosphorus Derivative.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: TRIETHYL PHOSPHONOACETATECAS: 867 – 13 – 0Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: TRIETHYL PHOSPHONOACETATE is an intermediate used in the manufacturing of fine chemicals ; used to homologate a carbonyl compound by conversion to an ethyl acrylate group using a Horner-Wadsworth Emmons reaction.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Chemical Properties Metric English Comments
Total Acid Number <= 2.0
<= 2.0
[mg KOH/g]; OPTI100
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
OSTM074
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Assay >98%
OPTI097
Color <100
APHA, OSTM010