Solvay RHODAPEX® ESY STD Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAPEX® ESY STD Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
I.N.C.I. Name: Sodium Laureth SulfateCAS: 68585-34-2Compatible with most surfactant solutions and water soluble polymers.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODAPEX ESY STD is used as primary foaming agent, shampoos, bath products, liquid soaps and related cosmetic products.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH 7.5 - 8.5
7.5 - 8.5
10% Solution; RP-0420
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clean clear liquid
RP-0064
Color <100
APHA, RP-0134
Composition Active
24.5-25.5%, EQ. WT. 346, RP-0027
Formalin
0.11-0.13%, RP-0197
Free Oil
0.65-2.5%, RP-17303
Sodium Chloride
<1%, RP-0098
Sodium Sulfate
<1.5%, RP-0555