Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay RHODACAL® LSS-40-A18 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODACAL® LSS-40-A18 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: X High-foaming detergent and emulsifier. Alkali stable. Also used as a foam booster, dispersant and wetter in dishwashing, car- wash products and general- purpose cleanersChemical Name: SODIUM ALPHA OLEFIN SULFONATE>CAS: 68439-57-6Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODACAL® LSS-40/A18 combines excellent detergency properties and foaming properties with high solubility and lower irritancy than sodium alkyl sulfates and sodium alkyl benzene sulphonates. It is recommended for the following: bubble baths, shampoos, fine fabric wash formulation, liquid soaps, and manual dishwash liquids.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
pH 5.5 - 7.0
5.5 - 7.0
10% Aqueous; RP-17601
Viscosity <= 200 cP
<= 200 cP
Optical Properties Metric English Comments
Gardner Color Number <= 4.0
<= 4.0
RP-17602
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Amber Liquid
RP-17620
Composition Active
38-40%, MW 324, RP-17102
EDTA Disodium
0.49-0.51%, RP-17648
Free Oil
<1.4%, RP-17607
Sodium Chloride
<1.0%, RP-17504
Sodium Sulfate
<1.5%, RP-17503
Total Plate Count
<10 cfu/g, RP-17635
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved