Solvay RHODACAL® A-246/L Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODACAL® A-246/L Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: X High-foaming detergent and emulsifier. Alkali stable. Also used as a foam booster, dispersant and wetter in dishwashing, car- wash products and general- purpose cleaners.Chemical Name: SODIUM C14-C16 SULFONATESolubility: Clear in a 10% water solution at 25°CAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODACAL A-246/L is an effective APE-free anionic surfactant for making small particle size acrylic, and styrene/acrylic latexes.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 40 %
40 %
pH 8.0 - 9.0
8.0 - 9.0
10% Solution; RP-17601
Viscosity <= 500 cP
<= 500 cP
RP-17619
Surface Tension 29 dynes/cm
29 dynes/cm
at CMC
Chemical Properties Metric English Comments
Ionic Impurities - Fe (Iron) <= 5.0 ppm
<= 5.0 ppm
RP-17610
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear Amber Liquid
Color <100
Klett, 5% Active, RP-17604
Composition Active
38-40%, EQ.WT 315, RP-17102
Formalin
0.13-0.27, RP-17612
Sodium Chloride
<1%, RP-17504
Sodium Sulfate
<2.0%, RP-17503
Total Plate Count
<10 cfu/g, RP-17635
Critical Micelle Concentration 0.0007
Ionic Charge Anionic