Material Notes:
Description: Cationic polymer providing good wet/dry combability properties. Imparts smooth feel, luster and detangling properties to the hair and smooth feel to the skin. Non dulling conditioning effect on fragile and fine hair. Reduces trans-epidermal water lossC.T.F.A. /I.N.C.I. Name: POLYQUATERNIUM – 2CAS: 68555 – 36 – 2Recommended use level: 0.4 - 2.5 %.Available in: Asia Pacific, Europe, Latin America and North AmericaReadily soluble in water in all proportionsApplications: Cationic polymer, easily dispersible in water and compatible in amphoteric surfactant systems. Highly substantive conditioning agent for skin and hair care products. Hair Care: in shampoos and hair conditioners it confers good wet-combing, dry-combing, and produces a soft natural feeling. Reduces electrostatic build-up (Flyaway). Skin Care: is highly skin substantive and provides soft feeling to the skin (liquid soaps, ...). Note: In formulating Mirapol A-15, it is necessary to dissolve the Mirapol A-15 in about 75% of the required water before addition of the remaining ingredients.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
pH 7.5 - 8.5
7.5 - 8.5
10% aq. Sol.; AN3401
Viscosity <= 3000 cP
<= 3000 cP
Processing Properties Metric English Comments
Moisture Content 34 - 38 %
34 - 38 %
AN3150
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear to cloudy amber viscous liquid
Color <1000
AN3013
Composition Active
62-66%, AN3150
Chloride
11-13%, AN3331
Dichloroethylether
<2 mg/kg, AN6032
Dioxanne
<5 mg/kg, AN6032
Turbidity <3.0 NTU
AN3900