Material Notes:
Description: MIRACARE LSC-217 is a high active surfactant base specially developed for use in the preparation of high foaming hair shampoos and skin cleanser systems. An optimized blend anionic, betaine and foam boosting alkanolamide surfactants, MIRACARE LSC- 217 readily yields completely formulated products with simple water dilution. The viscosities of the resulting formulas can then easily be adjusted with judicious electrolyte additions.I.N.C.I. Name: PROPRIETARY SURFACTANT BLENDAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: MIRACARE LSC-217 is a high active surfactant base specially developed for use in the preparation of high foaming hair shampoos and skin cleanser systems. An optimized blend anionic, betaine and foam boosting alkanolamide surfactants, MIRACARE LSC- 217 readily yields completely formulated products with simple water dilution. The viscosities of the resulting formulas can then easily be adjusted with judicious electrolyte additionsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 64 - 67 %
64 - 67 %
RP-17645
pH 6.5 - 7.5
6.5 - 7.5
10% Aqueous; RP-17601
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Viscous Hazy Liquid
RP-17620
Composition Active
44-46%, MW 382, RP-17501
Sodium Chloride
<1.5%, MW 58.5, RP-17504
Sodium Sulfate
<2.0%, MW 142, RP-17503
Unsulfated Matter
<2.0%, RP-17648