Material Notes:
Product Description: Mackpearl 202 is a high-active liquid pearling agent designed for easy dispersibility at ambient temperatures. Mackpearl 202 is added slowly to the batch with moderate agitation to obtain attractive pearlescence and stability. The amount of Mackpearl 202 will vary from 3 to 12% based on the pearl effect desired. A widely used liquid pearl based on EGMS. Usually used in lower solids anionic systems. This grade is preserved with DMDM Hydantoin. Infrared Spectrum: Matches StandardUses: Shampoos, Liquid Hand Soaps, Body Baths and Washes, Bubble Baths and Liquid DishwashInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Solids Content 40 - 43 %
40 - 43 %
Moisture Balance
pH 7.0 - 8.0
7.0 - 8.0
10% Aqueous
Processing Properties Metric English Comments
Shelf Life 48.0 Month
48.0 Month
Descriptive Properties Value Comments
Appearance Opaque
Composition Bacteria Counts
<10
Glycol Stearate
0.17
Preservative DMDM Hydantoin
0.0022