Solvay MACKAM® CB-35 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name MACKAM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay MACKAM® CB-35 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Mackam CB-35 is an alkyl betaine that finds uses in industrial applications as well as well as personal care products. Mackam CB-35 is stable at acid /alkaline pH and with hypochlorite/hydrogen peroxide. It is a biodegradable, high foaming and in personal care applications contributes to conditioning feel. Chemical Name: Alkyl-BetaineInfrared Spectrum: Match StandardUses: Hand soaps, Shampoos, Body wash, Foaming carpet cleaners, Acid cleaners, Liquid hand dishwashInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Solids Content 33 - 36 %
33 - 36 %
Oven
pH 6.5 - 8.5
6.5 - 8.5
Optical Properties Metric English Comments
Gardner Color Number <= 2.0
<= 2.0
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
Composition Sodium Chloride
5.6-6.2%
Total Plate Count
<10 cfu/g