Solvay MACKADET® DR-100M Surfactant

Category Fluid
Manufacturer Solvay
Trade Name MACKADET®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay MACKADET® DR-100M Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Mackadet® DR-100M is a concentrated blend of surfactants, which simply requires dilution and the addition of minor additives to produce a ready to package high foaming product. To achieve optimal results, conditioning agents and fragrance should be added to this base just prior to dilution. The viscosity may be adjusted to desired consistency with sodium chloride (to increase) or sodium xylene sulfonate (to decrease). Mackadet DR-100M contains no diethanolamides and low VOC and is preserved with DMDM Hydantoin. Uses: Shampoos, Hand Soap, Body Wash and Dish Soap.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Solids Content 40 - 43 %
40 - 43 %
Oven
pH 5.0 - 6.0
5.0 - 6.0
Viscosity 2000 - 5000 cP
2000 - 5000 cP
20% Viscosity, 1-2% NaCl
<= 6000 cP
<= 6000 cP
#3 SP @ 12 rpm
Thermal Properties Metric English Comments
Flash Point >= 200 °C
>= 392 °F
Optical Properties Metric English Comments
Gardner Color Number <= 3.0
<= 3.0
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
Composition 1,4 Dioxane
<15 ppm
Total Plate Count
<10 cfu/g
Preservative DMDM Hydantoin
0.0022