Solvay Isooctyl Acid Phosphate

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Isooctyl Acid Phosphate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: ISOOCTYL ACID PHOSPHATECAS: 27215-10-7 & 26403-12-3Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Isooctyl Acid Phosphate is employed in many different applications such as acid catalysts in coatings, dispersants, lubricants and antistatic agents in textile manufacture.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Chemical Properties Metric English Comments
Total Acid Number 280 - 330
280 - 330
[mg KOH/g]; RPC11017
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear, colorless liquid
Color <500
APHA, RPC-11004
Composition Diisoocyl HPO
55-67%, RPC92604
Isooctyl DIHPO
32-41%, RPC92604
Phosphorus
11.2-11.9%, RPCXRF02