Material Notes:
Identification: Dodecylphenol EthoxylateCAS: 9014-92-0Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL RC-620 is a low foaming rewetting agent for paper towels, tissue and semi-chemical corrugated media. Good also be used in textile application.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clean, clear to slightly hazy liquid
RP-0064
Cloud Point 38-42°C
1% Solution, RP-0124
Color <100
APHA, RP-0134
Neutralization Number <0.5 mg KOH/g
pH7, RP-0343