Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay IGEPAL® CO 997 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name IGEPAL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay IGEPAL® CO 997 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: NONYLPHENOXY POLY(ETHYLENEOXY)ETHANOL, BRANCHED, 70% ACTIVECAS: 68412-54-4; 7732-18-5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL© CO-977 is a versatile emulsion polymerization surfactant and latex post-stabilizer. IGEPAL© CO-977 can be used as both a sole-emulsifier and a co-emulsifier.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 70 - 73 %
70 - 73 %
CEM, 60% Power; RP-0528
Surface Tension 60 dynes/cm
60 dynes/cm
at CMC
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear liquid
at 35°C, RP-0064
Viscous Liquid
Tends to Solidify on Standing, at 25°C, RP-0064
Color <100
APHA, RP-0134
Critical Micelle Concentration 0.001
HLB number 19
Hydroxyl Number 12-15 mg KOH/g
Before water, RP-0245
Ionic Charge Nonionic
Moles of Ethylene Oxide 100
Neutralization Number <0.5 mg KOH/g
pH7, RP-0343