Solvay IGEPAL® CO 730 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name IGEPAL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay IGEPAL® CO 730 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic dispersant and emulsifier for cosmetic formulations.Identification: Nonoxynol-12CAS: 68412-54-4Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL CO-730 is a Nonionic co-emulsifier used in emulsion polymerization and also used as a wetting agent in different formulations. Hair Color Treatment, Hard Surface Cleaners, Laundry Detergent LiquidsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Surface Tension 39 dynes/cm
39 dynes/cm
at CMC
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Hazy to opaque liquid
May solidify on standing, RP-0064
Cloud Point 63-67°C
1% in 10% Salt Sol., RP-0124
Color <100
APHA, RP-0134
Critical Micelle Concentration 8E-05
HLB number 15
Ionic Charge Nonionic
Moles of Ethylene Oxide 15
Neutralization Number <0.5 mg KOH/g
pH7, RP-0343