Material Notes:
Description: "New ether carboxylate. Based on a fatty alcohol which is commonly available. Emulsifier and lime soap dispersant for metal working fluids."Identification: ALCOHOL ETHO-CARBOXYLATED ACID FORMAvailable in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Dispersible in water and aromatic solvents. Soluble in most polar solvents.Applications: Anionic emulsifier for Metal Working Fluids and lime soap dispersant. GEROPON HW 15 N can provide excellent hard water resistance to aqueous Metal Working Fluids.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
pH 1.6 - 2.8
1.6 - 2.8
10% in water; 540MA3C1E
Thermal Properties Metric English Comments
Pour Point 0.000 °C
32.0 °F
Flash Point >= 100 °C
>= 212 °F
Optical Properties Metric English Comments
Gardner Color Number <= 6.0
<= 6.0
540MA3C67
Chemical Properties Metric English Comments
Total Acid Number 61 - 71
61 - 71
[mg KOH/g]; 540MA3C21
Processing Properties Metric English Comments
Moisture Content 6.0 - 10 %
6.0 - 10 %
Karl Fisher; 540ME3C24
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Yellow liquid to gel
Composition Active
0.9
NaCl
<1.5%, 540MA3C10
Ionic Charge Anionic
Copyright © lookpolymers.com All Rights Reserved