Material Notes:
Description: DEXFLEX® 980HF is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact properties at low temperatures, and good paint adhesion with UV stability. Applications: Bumper fascias Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183
Linear Mold Shrinkage 0.0090 - 0.012 cm/cm
0.0090 - 0.012 in/in
as molded; ISO 294
0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
after bake; ISO 294
Melt Flow 21 g/10 min
21 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 0.900 GPa
131 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 18.0 J
13.3 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
44.4 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228