Material Notes:
Identification: DIMETHYL OCTADECYLPHOSPHONATECAS: 25371 – 54 – 4Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: DURAPHOS® 100 is a highly stable antiwear for oil and grease formulations Recommended for its high thermal and oxidative stability it is effective at low dosage in automotive gear, transmission fluids and in industrial lubricants.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Thermal Properties Metric English Comments
Melting Point 40.0 - 48.0 °C
104 - 118 °F
OPTI056
Chemical Properties Metric English Comments
Total Acid Number <= 20
<= 20
[mg KOH/g]; OPTI057
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance White waxy solid
Composition Total Phosphorus
8.3-8.8%, OPTI058