Solvay Chemicals SPG Barium Hydroxide Monohydrate

Category Ceramic
Manufacturer Solvay Chemicals
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals SPG Barium Hydroxide Monohydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Solvay
Descriptive Properties Value Comments
Appearance white crystals
Assay 0.99
Composition 15 ppm
Fe
Sieve Analysis 0
>1.4 nm
3-6%
<0.075 nm