Material Notes:
HFC SOLKANE 134a, a high purity gas liquefied under pressure, has a wide range of applications in the plastic foam sector (OCF,XPS, PU,PIR). CAS-No.: 811-97-2 / EC-No.: 212-377-0 / REACH Registration Number: 01-2119459374-33 Uses: Foaming agentsInformation provided by Solvay
Physical Properties Metric English Comments
Molecular Weight 102 g/mol
102 g/mol
Thermal Properties Metric English Comments
Melting Point -108 °C
-162 °F
Boiling Point -26.0 °C

@Pressure 0.1013 MPa
-14.8 °F

@Pressure 14.69 psi
Descriptive Properties Value Comments
Appearance compressed liquefied gas
Color colorless
Composition >99.5%
1,1,1,2 Tetrafluoroethane