Physical Properties Metric English Comments
Solids Content 20 %
20 %
Particle Size >= 50 µm
>= 50 µm
Viscosity 6.5 cP
6.5 cP
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month