Material Notes:
Flux/binder system to reduce flux fall-off and minimize dust formationUses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided by Solvay
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Solids Content 4.0 %
4.0 %
Vapor Pressure 0.0220 bar
16.5 torr
bibliographical ref.
Thermal Properties Metric English Comments
Boiling Point 100 °C
212 °F
bibliographical ref.
Descriptive Properties Value Comments
Composition 0.01
Organic
Explosion limit 0.013
Lower
0.095
Higher
Solid volume 3.9 l/100 kg
Viscosity 20 s 4 mm