Material Notes:
NOCOLOK® Precoating can be used in mixture with NOCOLOK® Flux or NOCOLOK® Zn Flux and water to improve adhesion of the flux coating. Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided by Solvay
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Viscosity >= 40 cP
>= 40 cP
Vapor Pressure 0.0220 bar
16.5 torr
bibliographical ref.
Thermal Properties Metric English Comments
Boiling Point 100 °C
212 °F
bibliographical ref.
Descriptive Properties Value Comments
Appearance Viscous liquid
Color milky
Explosion limit 0.013
Lower
0.095
Higher